Analisis Pendekatan Nilai %Ekstraksi Ore North Mainrigde Dengan Metode Bottle Roller Test Di PT. J Resources Bolaang Mongondow

Authors

  • Frederico Espinoza Rangan Program Studi Teknik Metalurgi, UPN "Veteran" Yogyakarta
  • Yogi Gautama Yanas PT. J Resources Bolaang Mongondow
  • Fahrul Rozzi Usman PT. J Resources Bolaang Mongondow

DOI:

https://doi.org/10.19184/jeneral.v5i1.45633

Keywords:

Bottle Roll Test, %Ekstraksi, Emas, Ore North Maindrigde

Abstract

The heap leach method is one of the cyanidation processes suitable for low-grade ore and PT J Resources Bolaang Mongondow uses this method in its processing. Column test is the most representative testwork of the heap leach process, but this testwork requires a long time so a faster testwork is needed and can provide %extraction value even though it is less representative and bottle roll test (BRT) is a solution for this. This study aims to estimate the % extraction obtained in cells by the BRT method. From the experimental results, it was obtained that the %extraction value of HG 01 samples at +12, +6, and -6 sizes was 67.1%, 79.2%, and 92.4%, respectively. for LG 02 samples of 68.3%, 81.5%, and 93.9%, for LG 03 samples of 54.5%, 90.6%, and 89.6%, respectively, these three samples are categorized as med-high extraction. While the LG 04 sample was 67.3%, 66.3%, 84.8% and categorized as low extraction.

Downloads

Download data is not yet available.

References

Marsden, J., & House, I. 2006. The chemistry of gold extraction. SME.
PT. JRBM. 2023. Data PT. J Resources Bolaang Mongondow.
Widara, M. R. 2017. Perbandingan Hasil Logam Emas Pada Pengolahan Bijih Emas Dengan Metode Sianida (Heap Leaching) Berdasarkan Perbedaan Ukuran Butir Umpan. ReTII.
Yannopoulos, J. C. 1991. The Extractive Metallurgy of Gold Extractive of Gold.